MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Astralloy A-514 Grade B High Yield Strength, Quenched & Tempered Alloy Steel Plate
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Fine grained, fully killed alloy steel used in applications where high strength, low weight and high impact values are required.
  • Quenched and tempered constructional alloy with high yield strength at 90 or 100 ksi minimum, width weldability and good toughness at low atmospheric temperatures.
  • Offers the optimum in strength, toughness, corrosion resistance, impact-abrasion resistance, and long term economy.
  • Used in components for earthmoving or transport equipment, booms, bucket parts for power shovels or cranes, penstocks, turbine scroll cases and unfired pressure vessels.
  • Not recommended for service at temperatures lower than -50°F or higher than 800°F.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 ksi
Tensile Strength, Yield 100 ksi
Bend Radius, Minimum 4.0 tPerpendicular to Grain Direction
 5.0 tParallel to Grain Direction
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 800 °F
Minimum Service Temperature, Air -50.0 °F
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 0.0050 %
Carbon, C <= 0.21 %
Chromium, Cr <= 0.65 %
Iron, Fe >= 96.7 %As Balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.25 %
Nickel, Ni <= 0.70 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.010 %
Titanium, Ti <= 0.040 %
Vanadium, V <= 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A516 Carbon Steel, Grade 70
Astralloy A-514 Grade H High Yield Strength, Quenched & Tempered Alloy Steel Plate
AISI 4140 Steel, oil quenched, 50 mm (2 in.) round [845°C (1550°F) quench, 540°C (1000°F) temper]
Astralloy A-514 Grade F High Yield Strength, Quenched & Tempered Alloy Steel Plate
ThyssenKrupp N-A-XTRA® M 700 Structural Steel

NNUCOR906 / 233180

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.