MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.

Polypropylene PPM H350 is characterized by high fluidity and is particularly suitable for injection molding applications. The material provides a good balance between stiffness and impact.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 96ISO 2039-2
Tensile Strength, Yield 32.0 MPaISO 527-2
Elongation at Yield 9.0 %ISO 527-2
Tensile Modulus 1600 MPaISO 527-2
Flexural Modulus 1500 MPaISO 179
Izod Impact, Notched (ISO) 2.50 kJ/m²ISO 180
Charpy Impact, Notched 3.00 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C120°C per hour; ISO 752
Vicat Softening Point 89.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 153 °C
@Load 1.02 kg
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical SEETEC H7700 Polypropylene, Homopolymer
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
Total PPM H250 Polypropylene, Homopolymer Medical Grade
Bamberger Polymers Bapolene® 4082 Polypropylene, Injection Grade
Borealis HH450MO Polypropylene

PTOTAL878 / 130603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.