MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Special Metals NIMONIC® Alloy PE11
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at temperatures to 1020°F (550°C). The high iron content provides good workability and also relatively high tensile ductility, especially after welding. Used for components of gas turbines. Standard product forms are round, flats, extruded section, plate, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy; DTD 5037; AFNOR Z8 NC D38
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 950 MPa
@Temperature 650 °C
Precipitation Hardened prior to test
 1060 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 700 MPa
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 680 MPa
@Strain 0.2 %,
Temperature 650 °C
Precipitation Hardened prior to test
Elongation at Break 20 %Precipitation Hardened
 15 %
@Temperature 650 °C
Precipitation Hardened prior to test.
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.021at 300 Oersted (23.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.436 J/g-°C
Melting Point 1280 - 1350 °C
Solidus 1280 °C
Liquidus 1350 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.70 - 1.0 %
Boron, B <= 0.0010 %
Carbon, C 0.030 - 0.080 %
Chromium, Cr 17 - 19 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.50 %
Iron, Fe 32 %As remainder
Manganese, Mn <= 0.20 %
Molybdenum, Mo 4.75 - 5.75 %
Nickel, Ni 37 - 41 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.015 %
Titanium, Ti 2.2 - 2.5 %
Zirconium, Zr 0.020 - 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NIMONIC® Alloy 86
Special Metals NIMONIC® Alloy 901
Special Metals NIMONIC® Alloy 105
Special Metals NIMONIC® Alloy 115
Special Metals NIMONIC® Alloy 263

NINC69 / 17419

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.