MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ 2000EZ is a high-heat PC/ABS resin delivering optimized performance for automotive interior component applications.

Benefits:

  • Easy flow, reduced scrap, and faster cycle times, while enabling thin wall part design for mass reduction
  • High-impact strength even at low temperature
  • High Heat resistance for demanding automotive interior components
  • Consistent natural white color produces high quality part appearance when used with color concentrates (self coloring) or Trinseo Color Masterbatch Technology
  • Low odor & VOC to meet all global Automotive OEM specifications
Applications:
  • Mid (floor) consoles
  • Instrument Panel components
  • Door panel trim
  • Pillars
  • Storage/load floors/glove box
Automotive Specifications:
  • 3M 11-0003-5762-1
  • CHRYSLER MS-DB-195 CPN2967
  • CHRYSLER MS-DB-195 CPN3401
  • CHRYSLER MS-DB-195 CPN4598
  • DAIMLER DBL 5404.29
  • GM GMW155819-ABS+PC-T3
  • RNPO AS33
  • TOYOTA TSM 5526G-2
  • VOLKSWAGEN TL 522 31-A
  • BMW GS 93016
  • CHRYSLER MS-DB-195 CPN3159
  • CHRYSLER MS-DB-195 CPN3408
  • DAIMLER DBL 5404.28
  • FORD WSS-M4D585-C1
  • GM GMW15581P-ABS+PC-T6
  • TESLA TM-1003 10/20
  • VOLKSWAGEN TL 522-31
  • VOLKSWAGEN TL 522-31-B

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183/B
Apparent Bulk Density 0.660 g/ccISO 60
Linear Mold Shrinkage 0.0040 - 0.0070 in/in
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
Spiral Flow 47.0 cm
@Temperature 260 °C
Melt Temp: 260°C, Mold Temp: 60°C, Injection Pressure: 1.8E+3 bar
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.0 MPaISO 527-2/50
Elongation at Break 120 %ISO 527-2/50
Tensile Modulus 2500 MPaInjection Molded, 1 mm/min; ISO 527-2
Flexural Modulus 2300 MPa2.0 mm/min; ISO 178
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -30.0 °C
Type 1, Edgewise, Notch A; ISO 179
 50.0 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 106 °CUnannealed; ISO 75-2/A
Vicat Softening Point 128 °CISO 306/B50
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 290 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 105 °C
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Mitsubishi Xantar® C CM 406 Polycarbonate
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR

PDWST085 / 142294

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.