MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Nylex™ 2185 NAT Polyamide + PP
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polypropylene (PP)

Material Notes:

Features:

  • Crack Resistance, Good
  • Dimensional Stability, Good
  • Impact Resistance, Good
  • Moisture Resistant
  • Processability, Good
  • Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Uses:

  • Electrical Parts
  • Housing, Electrical
  • Safety Equipment
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 0.970 g/cc0.970 g/ccASTM 792
    Water Absorption 0.65 %0.65 %ASTM D570
    Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
    Melt Flow 1.4 g/10 min1.4 g/10 minCond. Q; ASTM D1238
     4.7 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    4.7 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 40.1 MPa5820 psiASTM D638
    Elongation at Break 95 %95 %ASTM D638
    Flexural Strength 47.5 MPa6890 psiASTM D790
    Flexural Modulus 1.43 GPa207 ksiTangent; ASTM D790
    Izod Impact, Notched 0.908 J/cm1.70 ft-lb/in73°F; ASTM D256
    Gardner Impact 11.298 J8.3333 ft-lbASTM D3029
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 275 °C527 °FUnannealed; ASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FUnannealed; ASTM D648
     
    Processing PropertiesMetricEnglishComments
    Rear Barrel Temperature 205 °C401 °F
    Middle Barrel Temperature 208 °C406 °F
    Front Barrel Temperature 213 °C415 °F
    Nozzle Temperature 213 °C415 °F
    Mold Temperature 13.0 - 47.8 °C55.4 - 118 °F
    Injection Pressure 2.41 - 8.27 MPa350 - 1200 psi
    Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
     
    Descriptive Properties
    Injection RateModerate-Fast

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    A. Schulman Lucent TPP-310 Polypropylene, 10% Talc Filled, Impact Modified
    Ensinger TECAFINE™ PP Polypropylene (PP)
    Niche Polymer PPHM6BK Homopolymer PP

    PMULTI129 / 54033

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.