MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Luran® 378P G7 Styrene Acrylonitrile (SAN)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded, Glass Reinforced

Material Notes: Luran® 378P G7 is a glass fiber-reinforced grade (35% GF) of SAN with very high stiffness and low thermal coefficient of linear expansion. It features good chemical and weathering resistance and is suitable for extrusion and injection molding. Excellent mechanical strength, Excellent dimensional stability, Good heat resistance, Chemical resistance. Applications: Window frames, Precision parts, Machine construction

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.850 g/ccwith external lubricant
Density 1.36 g/ccISO 1183
Moisture Absorption at Equilibrium 0.25 %
@Temperature 23.0 °C
50% RH; ISO 62
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93
Ball Indentation Hardness 240 MPaISO 2039-1
Tensile Strength, Yield 110 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 12000 MPaISO 527
Flexural Strength 150 MPaISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
 4.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
Charpy Impact Unnotched 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 17.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 9500 MPaISO 899
Tensile Creep Modulus, 1000 hours 7500 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0070
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°CISO 11359
Thermal Conductivity 0.215 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 108 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 104 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 109 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CISO 294
Mold Temperature 40.0 - 80.0 °CISO 294
Injection Velocity 200 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® 358N SAN
INEOS Styrolution Luran® 388S Styrene Acrylonitrile (SAN)
INEOS Styrolution Luran® 368R Crystal Clear Transparent 77851 SAN
INEOS Styrolution Luran® 378P Crystal Clear Transparent SAN
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance

PSTYR9856 / 216083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.