BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical applications are pump housings, armatures, covers and boxes for use within the chemical industry. The chemical resistance of the material is a complex subject and exposure time, temperature and type of chemical media are important. The product is fire retardant and self-extinguishing.Information Provided by Menzolit |