Applications: Automotive Compounding Base, Industrial Parts Typical properties: SEETEC M1810 is a polypropylene block copolymer controlled rheology for injection molding applications. It exhibits a good balance of stiffness and impact strength. This grade meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact. Information provided by LG Chemical |