MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dover Chemical MAYCO BASE RP 8765 Dicarboxylic Acid Salt Based Compound Synthetic Corrosion Inhibitor
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mayco Base RP-8765 is a corrosion inhibitor formulated for use in synthetic and semi-synthetic metalworking coolants. It can be utilized in both oil-absorbing and oil-rejecting synthetic fluid types. It is completely water soluble in all proportions, yielding very light-colored transparent solution. As opposed to other corrosion inhibitors, Mayco Base RP-8765 also brings a slight amount of lubricity to the formulated product. Mayco Base RP-8765 can be formulated into: Synthetic rust preventatives for in-process protection. Rust inhibitors for coolant tank-side additions. Inhibition packages for synthetic and semi-synthetic fluids Used at 12% concentration in the following grinding coolant, Mayco Base RP-8765 exhibits complete rust protection to a 33:1 dilution in 100ppm water.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
@Temperature 15.6 °C
60/60°F
Density 8.83 lb/gal
pH 7.85% concentration
 8.0Neat
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 185[meqHCl/g]
 
Descriptive Properties
AppearanceClear Light Amber
Total Alkalinity20[meqKOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER147 / 217766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.