MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GRECO ISOTANE® 8201 Polyether TPU Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Characteristics: ISOTHANE® 8000 series products are polyether based engineering thermoplastic polyurethanes. They exhibit excellent tensile and flexural strength, toughness, abrasive resistance, good fatigue resistance, solvent resistance and maintenance of good physical properties under UV exposure. ISOTHANE® 8000 series can be injection molded extruded.

Application: Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products

Information provided by Great Eastern Resins Industrial Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ASTM D2240
Tensile Strength 83.0 MPa12000 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 1.57 GPa228 ksiASTM D638
Flexural Strength 108 MPa15700 psiASTM D790
Flexural Modulus 1.85 GPa268 ksiASTM D790
Izod Impact, Notched 1.08 J/cm
@Thickness 6.35 mm
2.02 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FASTM D648
Vicat Softening Point 112 °C234 °FASTM D1525
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRECO5199 / 282182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.