MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 1001 XV is a C4 Ziegler Natta LLDPE for power cable and Telecom jacketing. The grade contains a low level of antioxidants and has excellent Environmental Stress Crack Resistance (ESCR). Sufficient Carbon Black or UV Stabilizer should be added to meet cable jacketing specifications

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Stabilizer: Yes
Applications:
  • Halogen-free flame retardant (HFFR) compounds
  • LV thermoplastic jacketing
  • MV/HV thermoplastic jacketing
  • Telecom thermoplastic jacketing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.981 g/cc0.0354 lb/in³ExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 49
@Time 15.0 sec
49
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 19.3 MPa2800 psiASTM D638
Tensile Strength, Yield 11.7 MPa1700 psiASTM D638
Elongation at Break 830 %830 %ASTM D638
Elongation at Yield 20 %20 %ASTM D638
Flexural Modulus, 1% Secant 255 MPa37000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+15 ohm-cm7.00e+15 ohm-cmASTM D257
Dielectric Constant 2.22.2ASTM D150
Dielectric Strength 51.2 kV/mm1300 kV/inASTM D149
Dissipation Factor 0.000500.00050ASMT D150
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 120 °C<= 248 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adsyl 5 C 37 F ST Polyolefin
Versalis Flexirene® MR 50 U Linear Low Density Polyethylene
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
Equate EFDC-7087 LLDPE Film Extrusion Resin
Overview of materials for Low Density Polyethylene (LDPE), Film Grade

PEX99182 / 175418

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.