MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene YR92126 Polyolefin, Wire/Cable Grade
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: Petrothene YR92126 is a thermoplastic polyolefin-based, semiconductive, deformation resistant, black compound. YR92126 is selected for use as shielding and jacketing for medium voltage power cable. When properly extruded, cables produced with YR92126 will meet the requirements of AEIC CS 5-82 and ICEA S-66-524. Antioxidant has been added to ensure thermal stability during processing and enhance product performance. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D1505
Environmental Stress Crack Resistance >= 168 hour0 failures @ 7 days, cond. A; ASTM D1693
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240
Tensile Strength at Break 12.4 MPaASTM D638
Elongation at Break 220 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.0 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -25.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Feed Temperature 110 - 121 °C
Zone 2 132 - 143 °C
Zone 3 160 - 171 °C
Zone 4-x 160 - 171 °C
Adapter Temperature 160 - 171 °C
Die Temperature 160 - 171 °C
Melt Temperature 160 - 171 °C
 
Descriptive Properties
Processing MethodWire & Cable
Tensile Elongation at Break (% retained)90% ret., aged 7 days @ 100°C
Tensile Strength at Break (% retained)100% ret., aged 7 days @ 100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyolefin, Wire/Cable Grade
AlphaGary Garaflex™ O 9949 RA Olefinic Thermoplastic Elastomer
Teknor Apex HFFR 2002 Polyolefin, Halogen Free
Teknor Apex Flexalloy® 9607-96 Flexible Polyvinyl Chloride
Overview of materials for PVC, Wire and Cable Grade

PEQT8884 / 220518

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.