MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LCY Globalene TPV 1065A BK Thermoplastic Vulcanized Elastomers
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Globalene TPV 1065A BK can be processed by extrusion or molding for applications such as weatherstrip profile, seals, window gaskets and other soft touch articles.

Attributes:

  • Globalene TPV 1000 series is a fully vulcanized Thermoplastic Elastomers containing EPDM and PP.
  • It is designed for applications requiring long term sealing performance at elevated temperatures.
  • Suitable for injection molding, profile extrusion or re-compounding for plastics modification.
  • Conventional thermoplastic processing equipment can be used.
Applications: Globalene TPV has quality sealing property, good chemical and weathering resistance and electrical property that is suitable to replace main stream TPV, thermoset EPDM rubber, Styrene based TPEs, flexible PVC and other TPEs. It is an excellent choice for applications requiring flexibility in the following markets: automotive parts, appliance, business machines, construction, consumer products, and electronics.

Information provided by LCY Chemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 68
@Time 15.0 sec
68
@Time 0.00417 hour
Injection Molded; ISO 868
Tensile Strength at Break 8.00 MPa1160 psi500 mm/min; ISO 37
Elongation at Break 440 %440 %500 mm/min; ISO 37
100% Modulus 3.00 MPa435 psi500 mm/min; ISO 37
Tear Strength 20.0 kN/m114 pli500 mm/min; ISO 34-1
Compression Set  30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 43 %
@Temperature 125 °C,
Time 252000 sec
43 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °F
Brittleness Temperature -65.0 °C-85.0 °FISO 812
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 190 °C356 - 374 °FInjection
Middle Barrel Temperature 200 - 220 °C392 - 428 °FInjection
Front Barrel Temperature 200 - 220 °C392 - 428 °FInjection
Nozzle Temperature 200 - 220 °C392 - 428 °FInjection
Zone 1 180 °C356 °FExtrusion
Zone 2 190 °C374 °FExtrusion
Zone 3 200 °C392 °FExtrusion
Zone 4 210 °C410 °FExtrusion
Zone 5 210 °C410 °FExtrusion
Die Temperature 210 - 220 °C410 - 428 °FExtrusion
Melt Temperature 180 - 220 °C356 - 428 °FExtrusion
 200 - 220 °C392 - 428 °FInjection
Mold Temperature 30.0 - 55.0 °C86.0 - 131 °FInjection
Roll Temperature 20.0 - 50.0 °C68.0 - 122 °FExtrusion
Injection Pressure 4.80 - 6.90 MPa696 - 1000 psiInjection
Hold Pressure 2.10 - 4.10 MPa305 - 595 psiInjection
Back Pressure 0.0689 - 1.03 MPa10.0 - 150 psiInjection
Vent Depth 0.00254 cm0.00100 inInjection
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Cooling Time15-30 secInjection
Holding Time4-10 secInjection
Ozone ResistanceExcellent500 hr, 100 pphm O3 conc, ASTM D-1149
Screen Pack20-60 meshExtrusion
Screw>24:1L/D ratio
 3:1Compression ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLCY122 / 295665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.