Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CB 45G T 2003 (SC BLACK) is a 30% talc filled PP copolymer, with a good balance of flowability, impact strength and stiffness. Product is available as non color matched, black, pellet form. Applications: Exterior Automotive Applications. Information provided by LyondellBasell. |