MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mechanical properties, such as elongation, compression set, tensile and tear strength. The low density entails lower weight compared to the 600 and 660-series.

Information from Vita Thermoplastic Polymers (VTP).

Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
@Thickness 4.00 mm
ASTM D2240
Tensile Strength at Break 14.0 MPaASTM D638
Elongation at Break >= 600 %ASTM D638
100% Modulus 0.00500 GPa
@Strain 100 %
ASTM D638
300% Modulus 0.00600 GPa
@Strain 300 %
ASTM D638
Tear Strength 50.0 kN/mASTM D624
Compression Set 30 %
@Temperature 23.0 °C,
Time 259000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 210 °C
 
Descriptive Properties
Bonding to PPExcellent
Chemical ResistanceGoodExcluding organic solvents, aromatic and vegetable oils
ColorBlack
Weather ResistanceExcellentAir ageing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 662850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Black
ELASTO UK Dryflex® 660850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Natural
ELASTO UK Dryflex® 602850S SEBS Based Material, Filled Qualities, 85A Hardness, Black
ELASTO UK Dryflex® 600850S SEBS Based Material, Filled Qualities, 85A Hardness, Natural
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent

PVTC059 / 72128

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.