MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Channel Industries 1300 Barium Titanate Piezoelectric  (discontinued **)
Categories: Ceramic; Oxide; Titanium Oxide; Piezoelectric

Material Notes: Navy IV type

Modified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devices such as depth sounders and expendable hydrophones.

Uses of this grade include: Low Power Sonar; High Power Sonar; Depth Sounders

Data provided by Channel Industries, Inc.

Channel Industries was acquired by Piezo Kinetics in 2017.

Key Words: BaTiO3; Barium Titanium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 5.55 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 21.0 MPaDynamic tensile strength
 52.0 MPaStatic
 
Electrical PropertiesOriginal ValueComments
Curie Temperature >= 115 °C
Dielectric Constant 1350Free dielectric constant KT3
 1450KT1
Dissipation Factor 0.0080Low Field
Piezoelectric Longitudinal Coupling Factor, k33 0.45
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -56.0
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 245
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 12.2
Piezoelectric Planar Coupling Factor, kp -0.300
Piezoelectric Mechanical Q 600
Piezoelectric Shear Coupling Factor, k15 0.45
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 145
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -4.70
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 19.1
Piezoelectric Transverse Coupling Factor, k31 -0.180

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Channel Industries 300 Barium Titanate Piezoelectric
Harris Acoustic Sensors EC-21 Barium Titanate Piezoelectric
Barium Titanate, BaTiO3
Channel Industries 600 Barium Titanate Piezoelectric
American Elements Barium Titanate nanoparticles

CCHAN2 / 725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.