Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System. Tensile, Deformation, and Gel measured on a 95 phr S1042A / 5 phr S1000B system; and cured for 6 hours in water at 90 degree C. Brittleness Temperature is Information provided by PolyOne |