MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® VaporCoat® 2200R MVTR
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: MVTR, water and grease resistance coating

Usage: VaporCoat® 2200R is a coating which provides water and grease resistance and excellent MVTR properties on kraft liner and other substrates. When properly applied over a base coat, this repulpable coating is recommended as a replacement for some curtain coating applications, poly-laminated board and plastic bags.

Application Data: VaporCoat® 2200R is best applied by rod coater at a rate of 4-7 wet pounds per MSF and as a pre-applied coating or in-line at the wet end of the corrugator or by blade, flexo or gravure at the dry end of the corrugator.

Common uses include: Roll wrap for fine papers; Multi-wall bags; Produce and poultry boxes; Frozen meat patty boxes; Archival storage; and Corrosion-sensitive products

When manufactured in the USA product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1 (Restricted)

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 - 1.00 g/cc
pH 8.2 - 9.2
Brookfield Viscosity 100 - 600 cPSpindle # 3, rpm 60
Viscosity Measurement 15 - 19[sec], EZ cup, Cup # 3
 
Descriptive Properties
AppearanceOff-white liquid
Solids TypePolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui UNISTOLE™ P-801 Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ R-100K Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-902M Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-902 Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-401A Polyolefinic Primer/ Adhesive

WMICHEL206 / 135123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.