ELKON® 2110 is a sintered tungsten-silver material that is made into wire. This wire can be cold headed into rivet contacts or discs, which can be brazed, to rivets or other backings. ELKON® 2110 provides resistance to sticking and has uniform surface wear. Elkon® 2110 does not resist erosion nearly as greatly as other members of the tungsten-silver family. This material is used in automotive circuit protectors generally operating against a Molybdenum silver ELKON® mating contact. ELKON® 2110 is used in wall switches and thermostats such as blanket thermostats. Its uniform surface wear helps maintain a uniform calibration in thermostats.Information provided by NAECO, LLC. |