MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Edinburg Plastics DOG056 PA 6/6 Flame Retardant, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Appearance: Colors

Processing Methods: Injection

Applications: Flame Retardant

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.59 g/ccASTM D792-91
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19500 psiASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Yield Strength 28000 psiASTM D790
Flexural Modulus 1.30e+6 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 237 °CASTM D648
Flammability, UL94 5VA
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 249 - 260 °C
Middle Barrel Temperature 271 - 282 °C
Front Barrel Temperature 277 - 288 °C
Nozzle Temperature 277 - 288 °C
Melt Temperature 282 °C
Mold Temperature 60.0 - 88.0 °C
Drying Temperature 79.0 °C
Dry Time 4.00 - 8.00 hour
Moisture Content <= 0.20 %
Dew Point >= -40.0 °F
Back Pressure 40.0 - 100 psiLower is better
Screw Speed 30 - 70 rpmLower is better

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 203 FR XB Nylon 6/6 (PA), Glass Fiber - Flame Retardant - RoHS Compliant
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
Epsan Eplamid 66 GV0 30 NC Q1D0C001 Polyamide 66, Halogenated
Edinburg Plastics DOA006 PA 6/6 Flame Retardant

PEDIN024 / 183527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.