MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dynasol Calprene® 412 Thermoplastic Rubber SBS Dry
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Calprene 412 is a 69/31 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and has a radial structure.

This product is available in:

  • C 412 porous pellet
  • C 412M powder form dusted with amorphous silica

Applications:

  • Bitumen modification
  • Plastic modification

Information provided by Dynasol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.40 %ASTM D-5668
Viscosity 2300 cP
@Temperature 180 °C
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer)
Brookfield Viscosity 23100 cP25% toluene solution; MA 04-3-064
Viscosity Measure 28 cStToluene solution viscosity 5,23%; MA 04-3-003
Ash <= 0.35 %ASTM D-5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 31 %on polymer; ASTM D-5775
 
Mechanical PropertiesOriginal ValueComments
Penetration <= 50at 25°C dmm, Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-5-86
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air <= -30.0 °CCold Flexibility
Ring & Ball Softening Point >= 135 °CModified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-36
 
Descriptive Properties
Hunterlab color, max2
Insolubles in toluene, 325 mesh, % max0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Kibiton® PB-511 SBC
Chi Mei Kibiton® PB-585R SBC
Chi Mei Kibiton® PB-587 SBC
Dynasol Calprene® 411 Thermoplastic Rubber SBS Dry
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer

PDYNA46 / 34792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.