Properties and applications: ACEMATT 440 is an untreated extremely coarse-grained precipitated silica, particularly suitable for pigmented coatings systems with very low sheen (85° reflectometer value). This highly efficient matting agent is used in decorative and industrial coatings, based coats and thick-film coatings.Information provided by Evonik |