MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mo-Sci Corporation GL 1734 Glass
Categories: Ceramic; Glass

Material Notes: Applications: To seal ceramics and metals. Sealing glasses function as high-temperature sealant materials for solid oxide fuel cells (SOFCs) and other applications such as sodium-ion batteries.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.20 g/cc0.116 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.5 µm/m-°C8.06 µin/in-°Fcrystallized
Transformation Temperature, Tg 370 °C698 °F+/- 10°C
Softening Point 408 °C766 °FDilatometric +/- 10°C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 500 - 550 °C
@Time 3600 - 7200 sec
932 - 1020 °F
@Time 1.00 - 2.00 hour
Firing Temp. Heating/cooling rate: 3 to 10°C/min.
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.34 - 2.34 %0.34 - 2.34 %
B2O3 0.50 - 1.5 %0.50 - 1.5 %
BaO 9.06 - 13.06 %9.06 - 13.06 %
CaO 6.08 - 8.08 %6.08 - 8.08 %
K2O 3.25 - 5.25 %3.25 - 5.25 %
NaO2 3.47 - 6.47 %3.47 - 6.47 %
P2O5 44.37 - 50.37 %44.37 - 50.37 %
 
Descriptive Properties
Li2O (%)0.89 to 2.89
Sb2O3 (%)9.83 to 13.83
Tc620°C+/- 10°C
ZnO (%)8.64 to 12.64

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMOSCI9009 / 200224

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.