MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Saint-Gobain Furon® TR42 Thermally Conductive Acrylic Pressure-Sensitive Transfer Adhesive
Categories: Polymer; Adhesive; Tape; Thermoplastic; Acrylic (PMMA)

Material Notes: Description: A 2 mil thermally conductive acrylic pressure-sensitive transfer adhesive. Recommended uses: Excellent for flat surface bonding and laminating to other thermally-conductive materials. Application advantages: High peel strength adhesion to minimize air entrapment; Material can be pre-attached to a heat sink or other thermally conductive material; Adverse effects of surface roughness are minimized through a highly conformable pressure-sensitive adhesive; Flame-retardant version available; Available in slit-rolls or die cut shapes. All data based on a 0.002 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+14 ohm-cm2.10e+14 ohm-cmASTM D257
Dielectric Strength 23.6 kV/mm600 kV/inASTM D1000
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FASTM E1530
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Descriptive Properties
ColorWhite
Thermal Impedance @ 10 psi0.15°C in^2/WASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Grip™/Fastbond™ Water-based Adhesive 4224-NF Clear Industrial Adhesive
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer
Saint-Gobain Furon® TR45 Thermally Conductive Acrylic Pressure-Sensitive Transfer Adhesive
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer

PSTGQZ478 / 68992

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.