Ateva® 605A is a low melt index EVA Copolymer resin designed for extrusion and blow molding applications. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. A melt temperature in the 200-230°C range is recommended for this resin. Additives: Antioxidant Applications: Molding & Miscellaneous Information provided by Celanese Corporation. |
extrusion and blow molding applications |