MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Techmer ES HiFill® PA6 GF30 L 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight

Additive: Lubricant

Features: Lubricated

Processing Method: Injection Molding

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption  0.85 %
@Time 86400 sec
0.85 %
@Time 24.0 hour
ASTM D570
 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
 121121ASTM D785
Tensile Strength, Yield 162 MPa23500 psiASTM D638
 176 MPa25500 psiASTM D638
Elongation at Break 2.4 %2.4 %ASTM D638
 3.0 %3.0 %ASTM D638
Flexural Strength 214 MPa31000 psiASTM D790
 276 MPa40000 psiASTM D790
Flexural Modulus 1.03 GPa150 ksiASTM D790
 8.96 GPa1300 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 11.2 J/cm
@Thickness 3.17 mm
21.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 16.5 kV/mm420 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.4 µm/m-°C8.00 µin/in-°FASTM D696
 16.2 µm/m-°C9.00 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C420 °FUnannealed; ASTM D648
 218 °C425 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 6 GFR 30 NC HF Q1D002 Polyamide 6
Ashley Polymers Ashlene® 830LS-30G Nylon 6, 30% Glass Reinforced
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Domo TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0

PTPC0214 / 136152

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.