MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Omnix® 4050 High Performance (HPPA), Conditioned
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Conditioned data generated according to test method ISO 1110. MatWeb has a more thorough entry for dry samples.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.24 %
@Time 86400 sec
0.24 %
@Time 24.0 hour
ISO 62
Moisture Absorption 1.30 %1.30 %50% RH; ISO 62
Water Absorption at Saturation 3.8 %3.8 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 205 MPa29700 psiISO 527-2
Elongation at Break 2.7 %2.7 %ISO 527-2
Tensile Modulus 17.0 GPa2470 ksiISO 527-2
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²ISO 179
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Processing PropertiesMetricEnglishComments
Feed Temperature 80.0 °C176 °FInjection Hopper
Rear Barrel Temperature 260 °C500 °F
Middle Barrel Temperature 270 °C518 °F
Front Barrel Temperature 275 °C527 °F
Melt Temperature 270 - 310 °C518 - 590 °FInjection
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
176 °F
@Time 4.00 - 12.0 hour
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4363 / 280163

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.