MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Tenopom® B3 G30 NTLA010 PR334 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Medium Flow, Polyacetal Copolymer

Resin ID (ISO 1043): POM GF30
Processing: Injection Molding
Color: Natural

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 - 1.58 g/cc0.0564 - 0.0571 lb/in³ASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
Melt Flow 5.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 - 8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 28 - 32 %28 - 32 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 12 %12 %ASTM D638
Modulus of Elasticity 7.80 GPa1130 ksiASTM D790
Flexural Strength 150 MPa21800 psiASTM D790
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 - 167 °C327 - 333 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 169 °C336 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °C291 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FMolding
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 1.00 hour1.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL369 / 313277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.