MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex APEX® RE 9118A UV Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Form: Pellets

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
@Time 10.0 sec
ASTM D2240
Tensile Strength at Break 7280 psiASTM D638
Elongation at Break 130 %ASTM D638
Tensile Modulus 402000 psi0.2 in/min; ASTM D638
Flexural Modulus 410000 psiASTM D790
Izod Impact, Notched 2.90 ft-lb/in
@Thickness 3.17 mm
Injection Molded; ASTM D256
Dart Drop Total Energy 0.1625 ft-lb/mil
@Thickness 12.7 mm
Procedure A, TUP; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 61.3 °C
@Thickness 3.17 mm
Unannealed; ASTM D648
 69.2 °C
@Thickness 3.17 mm
Annealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 14.3 %
 
Descriptive Properties
AppearanceTransparent/slight blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0339 / 236830

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.