MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zeon Specialty Materials ZEONEX® 330R Cyclo Olefin Polymer
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Optical lens grade, very low birefringence

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Water Absorption <= 0.010 %ASTM D570
Melt Flow 11 g/10 min
@Load 2.18 kg,
Temperature 260 °C
JIS 6719
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaISO 527
Elongation at Break 3.0 %ISO 527
Flexural Modulus 3100 MPaISO 178
Izod Impact, Notched 13.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CASTM E831
Glass Transition Temp, Tg 123 °CJIS K7121
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.509ASTM D542
Transmission, Visible 92 %
@Thickness 3.00 mm
ASTM 1003
 
Descriptive Properties
Colorclear
Featureslow moisture absorption
Pencil Hardness3HJIS K5401
Primary MarketOptical Lens
Processing MethodInjection Molding
REACHYes
RoHSYes
Usesprism

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zeon Specialty Materials ZEONEX® 480R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® E48R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® 480 Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® K26R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® 790R Cyclo Olefin Polymer

PZEONC79 / 73138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.