MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AmodelĀ® AS-4133 L PPA, Conditioned
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Data for conditioned samples. MatWeb has a more thorough entry for dry samples.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 172 MPa24900 psiASTM D638
Elongation at Break 2.2 %2.2 %ASTM D638
Tensile Modulus 11.7 GPa1700 ksiASTM D638
Flexural Yield Strength 241 MPa35000 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Compressive Strength 172 MPa24900 psiASTM D695
Shear Strength 75.8 MPa11000 psiASTM D732
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VUL 746
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min0.709 in/minUL 746
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4093 / 279893

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.