MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Features

PBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hole products. Application in engineering, electrical and automotive industry. High mechanical properties also in conditioned state. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0092 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0168 cm/cmSTN 64 0808
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaSTN EN ISO 527-2
Elongation at Break 2.0 %STN EN ISO 527-2
Tensile Modulus 8000 MPaSTN EN ISO 527-2
Flexural Strength 160 MPaSTN EN ISO 178
Flexural Modulus 6500 MPaSTN EN ISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 50.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 7.00 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 7.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmSTN IEC 60093
Surface Resistance 1.00e+15 ohmSTN IEC 60093
Dielectric Strength 30.0 kV/mmSTN IEC 60243
Comparative Tracking Index 350 VSTN 34 6468
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 - 220 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °CSTN EN ISO 75/A
Vicat Softening Point 200 °CB; STN EN ISO 306
Flammability, UL94 V-0
Glow Wire Test 960 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 280 °C
Mold Temperature 50.0 - 90.0 °C
Drying Temperature 120 °C
Dry Time 4 hour
Moisture Content 0.050 %STN EN ISO 960
Injection Pressure 60.0 - 100 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Mitsubishi Novaduran® 5830GN6-40 Polybutylene Terephthalate
Evonik Vestodur® X9405 30% Glass Reinforced, Self Extinguishing PBT

PPLACO106 / 106984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.