MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Pyro-Bloc® EES System R Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: The Pyro-Bloc Electric Element Support (EES) System is a complete engineered package which includes Pyro Bloc Y modules, heating elements, hanging systems, and detailed drawings, that are a cost-effective method of hanging electric heating elements from Pyro-Bloc modules. EES system was patented over 20 years ago on the pre-embedded tubes, located within a ceramic fiber module, and the supporting hooks and washers. Applications: The type of furnace plays an important role in element orientation and manner of installation. For example, a bell furnace that is constantly moved would be designed much differently than a stationary pit furnace. Other furnaces requiring special consideration include car bottoms, tip-ups, and furnaces that see vibration, such as from roller rails.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³
 0.192 g/cc0.00694 lb/in³
 0.240 g/cc0.00867 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 10 kg/m3; ASTM C201
 0.0700 W/m-K
@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 12kg/m3; ASTM C201
 0.0700 W/m-K
@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 15 kg/m3; ASTM C201
 0.120 W/m-K
@Temperature 538 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 15 kg/m3; ASTM C201
 0.140 W/m-K
@Temperature 538 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 12kg/m3; ASTM C201
 0.150 W/m-K
@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 10 kg/m3; ASTM C201
 0.210 W/m-K
@Temperature 816 °C
1.46 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 15 kg/m3; ASTM C201
 0.240 W/m-K
@Temperature 816 °C
1.67 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 12kg/m3; ASTM C201
 0.260 W/m-K
@Temperature 816 °C
1.80 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 10 kg/m3; ASTM C201
 0.310 W/m-K
@Temperature 1093 °C
2.15 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 15 kg/m3; ASTM C201
 0.350 W/m-K
@Temperature 1093 °C
2.43 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 12kg/m3; ASTM C201
 0.390 W/m-K
@Temperature 1093 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 10 kg/m3; ASTM C201
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1204 °C2199 °FContinuous Use
 1316 °C2401 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 47 %47 %
SiO2 53 %53 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax PC Series™ PC Max™ Paper Ceramic Fiber Filtration Media
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material
Pyrotek Grade 1250 Ceramic fiber paper
Morgan Advanced Ceramics Thermo-Bloc Modules Ceramic Fiber Thermal Ceramic
Morgan Advanced Ceramics Pyro-Bloc® Module HS Thermal Ceramic

CMORF70126 / 203424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.