MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DOWSIL™ MS-0002 Optical Grade Moldable Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: LED lighting grade. DOWSIL™ silicone optical resins help increase design freedom and energy efficiency from high-performance buildings to outdoor-area illumination to advanced automotive styling. Compared to organic options, these specialty silicone liquid resins can maintain outstanding optical properties without yellowing with age under high temperatures.

Product applications:

  • Optical components
Key Features:
  • Fast curing
  • Translucent

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
Tensile Strength 9.00 MPaASTM D412
Elongation at Break 270 %ASTM D412
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 75 %
@Thickness 3.20 mm,
Wavelength 450 nm
 89 %
@Thickness 3.20 mm,
Wavelength 760 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWSIL™ MS-4007 Optical Grade Moldable Silicone
Dow DOWSIL™ MS-1003 Optical Grade Moldable Silicone
Dow DOWSIL™ MS-4002 Optical Grade Moldable Silicone
Dow DOWSIL™ MS-2002 Optical Grade Moldable Silicone
Dow DOWSIL™ MS-1002 Optical Grade Moldable Silicone

PDOW9964 / 233167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.