MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Braskem PIB 30 Polyisobutene Aliphatic Mono-olefin
Categories: Polymer

Material Notes: PIB 30 is obtained by polymerization of an isobutene rich stream with specific catalysts. Product is composed predominantly of aliphatic mono-olefins. It is clear, bright and free from sediments or suspended matter. PIB 30 is a non-toxic polymer and has NSF certification. It can be used in lubricants and synthetic oils formulation, including for food grade and pharmaceutical grade. PIB 30 is also applied in cosmetics as lip-gloss and in formulations of stretch film.
Applications: Lubricants, adhesives, cosmetics, stretch films.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D4052
Viscosity Measurement 186186Viscosity Index; ASTM D2270
Viscosity Measure  630 cSt
@Temperature 100 °C
630 cSt
@Temperature 212 °F
ASTM D445
 19500 cSt
@Temperature 37.8 °C
19500 cSt
@Temperature 100 °F
ASTM D445
Molecular Weight 1300 g/mol1300 g/molMn; Braskem Test-GPC
ASTM Color 5050Pt/Co; ASTM D1209
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.010<= 0.010mg KOH/g; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point 3.00 °C37.4 °FASTM D97
Flash Point 190 °C374 °FASTM D92
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 0.016 %0.016 %ASTM D5808
H2O, Water 0.0040 %0.0040 %ASTM D6304
Sodium, Na <= 0.00020 %<= 0.00020 %ASTM D4951
 
Descriptive Properties
Bromine Number (g Br2/100g)14ASTM D1159
Polydispersity Index (Mw/Mn)1.8Internal Method-GPC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS689 / 314082

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.