MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C96970, TX00 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Spinodal Hardened-Low Strength (ATLS)

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld; Good Suitability – Capacity for Being Hot Formed, Capacity for Being Cold Worked

Common Fabrication Processes: Casting; Drawing; Forming and Bending; Machining

Typical uses: Bearings; Bushings; Connectors; Plastic molding tooling; Retaining Rings; Valves; Wear Plates

Applicable Specifications: As Continuous Cast – ASTM B505/B505M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27
Tensile Strength 105 - 115 ksi
 110 ksiTypical
Tensile Strength, Yield 90.0 - 100 ksi0.2% Offset
 95.0 ksi0.2% Offset, Typical
Elongation at Break >= 3.0 %
Compressive Yield Strength 95.0 ksi
Poissons Ratio 0.30
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000132 ohm-cm13% IACS
Magnetic Permeability 1.001
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 100 °C
 9.50 µin/in-°F
@Temperature 20.0 - 200 °C
 9.70 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0910 BTU/lb-°F
Thermal Conductivity 30.0 BTU-in/hr-ft²-°F
Melting Point 1697 - 2012 °F
Solidus 1697 °F
Liquidus 2012 °F
Annealing Point >= 1400 °F
 
Processing PropertiesOriginal ValueComments
Solution Temperature >= 700 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 82.4 - 86 %As Balance
Iron, Fe <= 0.50 %
Lead, Pb <= 0.020 %
Magnesium, Mg <= 0.15 %
Manganese, Mn <= 0.30 %
Nickel, Ni 8.5 - 9.5 %
Niobium, Nb (Columbium, Cb) <= 0.10 %
Tin, Sn 5.5 - 6.5 %
Zinc, Zn <= 0.50 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC96970x1 / 292639

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.