MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polymer of choice for applications where softness, flexibility and polarity are required. LOTRYL® 20 MBG 08 contains slip and anti-block additives at the level required for extrusion coating process and fast sealing operations.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/cc
@Temperature 23.0 °C
ISO 1183
Methyl Acrylate Content 18 - 21 %IRTF (internal)
Melt Index of Compound 7.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ASTM D2240
Tensile Strength at Break 10.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
Flexural Modulus 20.0 MPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 °CDSC
Vicat Softening Point 48.0 °C
@Load 1.02 kg
ASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate

PARKG202 / 80068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.