MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-7106 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Feature:
  • Will not warp or bow
  • Chemically inert
  • Dimensionally stable
  • Grain-free stock material
  • Fine-cell structures
  • Closed-cell
  • Easily bonded and finished with a wide variety of adhesives and coatings
  • Low densities can be hand carved and shaped easily with common woodworking tools
  • Higher densities are available for CNC work where more accuracy is desired
  • Custom sizes available
Applications:
  • Proof stock
  • Composite core
  • Prototype models
  • Styling models
  • Tooling aids
  • Check fixtures
  • Mold patterns
  • Foundry patterns
  • Decorative trim

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 7.5cut foam surface; ASTM D2240
Tensile Strength 147 psiParallel to Rise; ASTM D1623
 158 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 168 psiRise Parallel to Beam Thick.; ASTM D790
 169 psiRise Parallel to Test Span; ASTM D790
Flexural Modulus 6186 psiRise Parallel to Test Span; ASTM D790
 6208 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 77.0 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 90.0 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 149 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 168 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
Compressive Modulus 2855 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 3437 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 4229 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 5288 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Thermal Conductivity 0.214 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 246 °FASTM E1824
 
Descriptive Properties
Tumbling Friability (%)6.520 mins at 60 rpm, ASTM C421
Water Absorption0.017 lbs/ft²ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3710 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3804 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-7110 Polyurethane Foam

PGENR045 / 186831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.