MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are required at both low and high temperatures (up to 190°C). This all-liquid formulation contains no solvents, and is easily mixed, handled and applied at room temperature, however a final elevated temperature cure step is REQUIRED for satisfactory bonds. Fully cured TRA-BOND 2211 develops strong, tough bonds for a wide range of materials which includes most metals, glass, ceramics, and many rigid plastics. It has excellent impact and thermal shock resistance, low permeability to gases and vapors, and outstanding resistance to water, weather, oxygen and ozone, most petroleum fuels and lubricants, mild acids and alkalis, and many other organic and inorganic compounds. An additional post-cure of 4 hours at 125°C is recommended when application temperatures higher than 125°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccMixed
Viscosity 2000 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Tensile Strength, Yield 8000 psi
Elongation at Yield 3.0 %
Adhesive Bond Strength 1050 psiLap shear, alum to alum, @ 165°C
 2000 psiLap shear, alum to alum, @ 125°C
 2500 psiLap shear, alum to alum, @ 25°C
Izod Impact, Notched 0.500 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+15 ohm-cm
 1.40e+12 ohm-cm
@Temperature 150 °C
Dielectric Constant 4.2
@Frequency 1000 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour12hrs @ 25°C + 2hrs @ 65°C + 2hrs @ 90°C
Pot Life 300 min
 
Descriptive Properties
Color Amber
Mix Ratio, parts by weight100/20Resin/Hardener
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive
Tra-Con Tra-Bond 161-3 Temperature Resistant Epoxy Adhesive

PTRAC060 / 70988

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.