MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Osprey H-C22 Nickel Alloy Powder
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Particles produced by gas atomization are spherical and can be produced in various sizes to accommodate various processing/printing techniques such as metal injection molding (MIM), additive manufacturing, plasma/thermal spray, or hot isostatic pressing (HIP).

Information provided by Sandvik Osprey.

Key Words: UNS N06022
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 21.5 %
Cobalt, Co <= 2.5 %
Iron, Fe 5.0 %
Manganese, Mn 0.70 %
Molybdenum, Mo 13 %
Nickel, Ni 39 %As Balance
Silicon, Si 0.40 %
Tungsten, W 4.0 %
Vanadium, V <= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy
Kennametal Stellite Nistelle C22 Nickel Superalloy
Polykemi AB SCANAMID 66.6 C22^E F Nylon 66/6, Modified
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated

NSANDV9924 / 220772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.