MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik Europlex® PPSU Polyphenylsulfone Engineering Plastic  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Description: EUROPLEX® PPSU is a sheet material distinguished by its special combination of properties:
  • high heat distortion temperature up to 190° C in permanent service
  • EUROPLEX® PPSU has outstanding mechanical properties over a wide temperature range (also at very low temperatures)
  • EUROPLEX® PPSU shows ggod chemical resistance for an amorphous material
  • Parts made of EUROPLEX® PPSU can be sterilized by all conventional methods, particularly by superheated steam at 2,000 cycles or more, also in combination with morpholine
  • EUROPLEX® PPSU therefore shows very particularly good resistance to hydrolysis
  • EUROPLEX® PPSU is inherently flame-retarded. Its rating to UL94:VO at 1.6 mm thickness stands for very good fire behavior
  • EUROPLEX® PPSU is physiologically unobjectionable and easily meets FDA and USP requirements for food contact and medical applications
  • Available in the form of transparent or opaque sheets in thicknesses of 0.8 to 6.0 mm
  • Sheets made from this material are mainly processed into medical containers for use in hospitals. Beside this EUROPLEX® PPSU sheets are more and more used in industrial plants and machines

Information provided by degussa.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527-2/1A/5
Modulus of Elasticity 2.34 GPaISO 527-2/1A/1
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 3.12 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 °CPermanent
Vicat Softening Point 207 °CISO 306/850
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Overview of materials for Polyphenylsulfone (PPSU)
CENTROPLAST CENTRO HPM Polyphenylensulfone
Evonik Europlex® PPSU High Performance Sheet
GEHR Plastics PPSU Polyphenylenesulfone

PHUK010 / 47144

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.