MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chi Mei Acryrex® CM-211 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes:
    Features:
  • Good Weather Resistance
  • High Clarity
  • High Flow
  • High Gloss
  • High Heat Resistance
  • High Viscosity
    Uses:
  • Containers
  • Cosmetics
  • Household Goods
  • Knobs
RoHS Compliant

Appearance: Clear/Transparent

Forms: Pellets

Processing Method: Extrusion and Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.700 g/ccApparent; ASTM D1182
 1.19 g/ccASTM D792
Water Absorption 0.30 %Equilibrium; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cmASTM D955
Melt Flow 16 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84
@Thickness 6.35 mm
6 mm/min; ASTM D785
Tensile Strength, Yield 63.4 MPa
@Thickness 3.18 mm
6 mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.18 mm
2.8 mm/min; ASTM D638
Flexural Strength 91.0 MPa
@Thickness 6.35 mm
ASTM D790
Izod Impact, Notched 20.0 J/m
@Thickness 6.35 mm
ASTM D256
Impact 2.0Impact Flexural Test Notched (KJ/m²)
 18Impact Flexural Test Unnotched (KJ/m²)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.7ASTM D150
Dielectric Strength 787 kV/inASTM D149
Dissipation Factor 0.19ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.35 mm
ASTM D648
Vicat Softening Point 102 °C50°C/hr; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Transmission, Visible 92 %
@Thickness 80.8 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 190 °C
Middle Barrel Temperature 195 - 215 °C
Front Barrel Temperature 190 - 210 °C
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 70.0 - 75.0 °C
@Time 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Acryrex® CM-205 PMMA
Chi Mei Acryrex® CM-207 PMMA
Chi Mei Wonderlite® PC-115 Polycarbonate
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin

PCHI945 / 109433

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.