MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes:

Data provided by the manufacturer, Amoco Corporation.

AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high tensile strength, high flexural modulus, low warpage, excellent dimensional stability, and low moisture absorption. This grade was designed specifically to be cost effective when high stiffness, good dimensional stability, and superior electrical properties are required. With a comparative tracking index of 450 volts and a deflection temperature of 505°F (263°C), this resin is a potential thermoset replacement in many electrical applications. Potential applications for AMODEL AF-1550 V0 resin include electrical relays, housings, motor starters, contactors, circuit breakers, and terminal blocks. This grade of AMODEL resin can also withstand the demanding vapor phase and infrared reflow soldering processes commonly used in the electronics industry for connectors and devices requiring surface mount technology.

This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

MatWeb has an entry for this material dry as molded.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.82 g/ccdry as molded
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 116 MPaASTM D638
Elongation at Break 1.0 %ASTM D638
Tensile Modulus 16.5 GPaASTM D638
Flexural Yield Strength 177 MPaASTM D790
Flexural Modulus 14.1 GPaASTM D790
Izod Impact, Notched 0.590 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.6
@Frequency 1e+6 Hz
ASTM D150
 4.7
@Frequency 100 Hz
ASTM D150
Dissipation Factor 0.018
@Frequency 100 Hz
ASTM D150
 0.026
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 243 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 321 - 338 °CInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
MTI ThermoStran® PPA-50G Long Glass Fiber Compound
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Avient Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)

PSOLVT36 / 21332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.