MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum LM6 As Manufactured, Gravity Die Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: LM6 is a corrosion resistant aluminum casting alloy with average durability and strength, and with high impact strength and ductility.

Applications: general, electrical, marine, intricate shaped castings, and building cladding panels

Key Words: Al Si12, BS 1490, LM 6; Aluminium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.68 g/ccAA 360.0
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 190 MPa
Elongation at Break 7.0 %5.65 vSo
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 84.95 - 87.95 %As remainder
Copper, Cu 0.10 %
Iron, Fe 0.60 %
Lead, Pb 0.10 %
Magnesium, Mg 0.10 %
Manganese, Mn 0.50 %
Nickel, Ni 0.10 %
Other, each 0.050 %
Other, total 0.15 %
Silicon, Si 10 - 13 %
Tin, Sn 0.050 %
Titanium, Ti 0.20 %
Zinc, Zn 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum LM6 As Manufactured, Sand Cast
Aluminum 413.0-F Die Casting Alloy
Aluminum 384.0-F Die Casting Alloy
Aluminum A413.0-F Die Casting Alloy
Aluminum LM2 As Manufactured, Pressure Die Cast

MAL09 / 10254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.