MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

UBE UBEPOL VCR® 800 Synthetic Polybutadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics: Broad molecular weight distribution type (Matrix BR). Improve extrusion characteristics of VCR450. Applications: Tires for passenger cars, trucks, buses, construction machinery, motorcycles and bicycles. Various industrial products such as polystyrene modifier, conveyor belts, hoses, rubber isolators and casters. Commodities such as shoe soles and golf balls.

UBEPOL VCR® consists of high-cis BR and high-crystalline syndiotactic polybutadiene resin which is a special type of polymer alloy. UBEPOL VCR® can contribute to produce various advantages: to increase hardness, modulus of rubber product without adding filler. To reduce the volume or weight of rubber product by utilizing its reinforcing effect. To improve extrusion properties (extrusion output and dimensional stability) and roll mill shrinkage.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/cc
Mooney Viscosity  40
@Temperature 100 °C
40
@Temperature 212 °F
ML1+4
 61
@Temperature 100 °C
61
@Temperature 212 °F
Compound. ML1+4. ASTM D3189
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666Curing time: 50 min
Tensile Strength 16.7 MPa2420 psi
Elongation at Break 380 %380 %
100% Modulus 2.90 MPa421 psiCuring time: 50 min
200% Modulus 7.40 MPa1070 psiCuring time: 50 min
300% Modulus 13.1 MPa1900 psiCuring time: 50 min
Rebound 49 %49 %BS. Curing Time: 50 min
Tear Strength 61.0 kN/m348 pliCuring time: 50 min
Abrasion 8888Lambourn. Index. Slip rate 60%. Curing time: 50 min
 9090Lambourn. Index. Slip rate 20%. Curing time: 50 min
 230230Pico. Index. Curing time: 50min
Compression Set 25 %25 %Curing time: 50 min
 
Descriptive Properties
Anti-OxidantNon-staining
Curing Characteristics10.1MH (dN*m). ASTM D3189
 12.6Tc(90) min. ASTM D3189
 2.1ML (dN*m). ASTM D3189
 3Ts1 min. ASTM D3189
 8.8Tc(50) min. ASTM D3189
Cut Generation (cycles)>30 e4Curing time: 50 min
Cut Growth Resistance (cycles)14000Cut length ; from 2mm to 15mm. Curng time: 50 min
Heat Build Up30°CDelta T
Heat Build Up (%)9P.S
Microstructure1Trans. % wt. Microstructure of matrix polymer.
 1Vinyl. % wt. Microstructure of matrix polymer.
 98Cis. %wt. Microstructure of matrix polymer.
n-Hexane Insoluble (%wt)5.3SPB content in VCR
Package35 kg bale

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9804 / 287267

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.