MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical HIPS 501S PS, Impact Modified
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: Injection Molding, PS, General Purpose, Impact Modified

Application: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yogurt Receptacle

CAS: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 19 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 80 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 99ASTM D785
Tensile Strength, Yield 270 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 59 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Yield >= 5.0 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Tensile Modulus 18000 kg(f)/cm²
@Thickness 3.20 mm
1mm/min; ASTM D638
Flexural Yield Strength 430 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Flexural Modulus 22000 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 6.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 8.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 12.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Strength 44.0 kV/mm
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 V
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 87.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
Flammability, UL94 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 170 - 190 °CInjection Molding
Middle Barrel Temperature 180 - 200 °CInjection Molding
Front Barrel Temperature 190 - 210 °CInjection Molding
Nozzle Temperature 190 - 220 °CInjection Molding
Melt Temperature 190 - 220 °CInjection Molding
Mold Temperature 40.0 - 70.0 °CInjection Molding
Drying Temperature 80.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution PS 476L HIPS
LG Chemical 60HR HIPS
LG Chemical 501S-S HIPS
LG Chemical 60HR-G HIPS
Daicel STYROL® GH10 HIPS

PLAY618 / 148628

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.