MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Radici Radilon® S RCP4015LK 100 NT Nylon 6, 40% Glass/Mineral Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced; Nylon 6, Heat Stabilized

Material Notes: PA6 40% glass fiber and mineral filler reinforced injection molding grade. Heat stabilized. Natural color. Suitable for parts requiring improved stiffness and dimensional stability, reduced shrinkage and low warpage.

ISO 1043: PA6-T (GF+MX)40

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by RADICI High Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccDAM; ISO 1183
Water Absorption 6.50 %
@Thickness 2.00 mm
Immersion; ISO 62
Moisture Absorption 1.60 %
@Thickness 50.8 mm
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00300 cm/cmMelt temp: 280°C; Mold temp: 80°C; Cavity Pressure: 60 MPa; ISO 294-4
Linear Mold Shrinkage, Transverse 0.00500 cm/cmMelt temp: 280°C; Mold temp: 80°C; Cavity Pressure: 60 MPa; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaDAM, 5 mm/min; ISO 527-2/1A
Elongation at Break 2.60 %DAM, 5 mm/min; ISO 527-2/1A
Tensile Modulus 11400 MPaDAM, 1 mm/min; ISO 527-2/1A
Flexural Strength 215 MPaDAM, 2 mm/min; ISO 178
Flexural Modulus 11000 MPaDAM, 2 mm/min; ISO 178
Charpy Impact Unnotched 22.0 kJ/m²DAM; ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm500V, Conditioned; IEC 62631-3-1
 1.00e+15 ohm-cm500V, DAM; IEC 62631-3-1
Surface Resistance 1.00e+10 ohm500V, Conditioned; IEC 62631-3-2
 1.00e+12 ohm500V, DAM; IEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75/2Af
Vicat Softening Point 210 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior Flammability; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 290 °CInjection
Mold Temperature 70.0 - 90.0 °CInjection
Drying Temperature 80.0 °Cdesiccant drier
Dry Time 2.00 - 4.00 hourdesiccant drier
Moisture Content <= 0.150 %
Dew Point -20.0 °Cdesiccant drier
 
Descriptive Properties
Injection Molding Injection SpeedMedium-high
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6231 / 327826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.