MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Applications:
  • Large blow molded containers for applications which require maximum toughness
  • 220 liter drums for chemicals

Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ISO 1872/1
ESCR, Bottle >= 200 hour
@Temperature 50.0 °C
>= 200 hour
@Temperature 122 °F
BP 13C/25
Melt Flow 0.010 g/10 min
@Load 2.16 kg
0.010 g/10 min
@Load 4.76 lb
ISO 1133
High Load Melt Index 2.0 g/10 min
@Load 21.6 kg
2.0 g/10 min
@Load 47.6 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiBP 13B/1
Elongation at Break 870 %870 %BP 13B/1
Flexural Modulus 1.10 GPa160 ksiISO 178-1975
Charpy Impact, Notched NBNBISO 179

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova 5420 High Impact Polystyrene
Kazanorgsintez PE2NT75-15 High Density Polyethylene for Blow Molding
LG Chemical LUTENE-H XL1800 HDPE
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene
Total 56020 S XP High Density Polyethylene - Blow Molding

PSIDP11 / 67706

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.