MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Matexcel MCP-005 Activated Carbon Cloth/Fiber
Categories: Other Engineering Material

Material Notes: Activated carbon fiber has a large number of micropores on the surface of the fiber, which is easy to adsorb, and the adsorption and desorption speed is fast. It can withstand higher concentrations of strong acid (hydrochloric acid) and strong alkali (potassium hydroxide and sodium hydroxide), and can withstand 500 degrees of burning in the air and 200 degrees of water heat in strong acid and alkali. The macroscopic appearance is cloth-like, and it can also be made into fiber.

Morphology: Cloth/Fiber

Key Words: Synonyms: Activated Carbon Cloth/Fiber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewSpecific surface area (BET): 1300-1400g/m2 Static benzene adsorption: 45-50% Iodine value (Iodine value): 1300-1400mg/g Hole Volume: 0.8-1.2ml/g Mean pore size: 1.7-2nm Fire point (Fire point): above 500?

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK2022 / 300653

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.