MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Baydur® 684 Polyurethane Structural Foam RIM, Density 30 pcf
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Baydur 684 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process.

Properties / Applications: Baydur 684 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process. The system is supplied as two reactive liquid components. Component A is a polymeric diphenylmethane diisocyanate (PMDI), and Component B is a formulated polyol system containing no CFC- or HCFC-blowing additives. The Baydur 684 system is used for applications requiring high compression strength foams, filling cavities and/or producing foam cores for overmolding. As with any product, use of the Baydur 684 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccPolyol
 1.24 g/ccIsocyanate
Viscosity 200 cPIsocyanate
 900 cPPolyol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
@Thickness 12.7 mm
ASTM D2240
Tensile Strength at Break 9.17 MPa
@Thickness 12.7 mm
ASTM D638
Flexural Strength 18.6 MPa
@Thickness 12.7 mm
ASTM D790
Flexural Modulus 595 MPa
@Thickness 12.7 mm
ASTM D790
Compressive Strength 14.0 MPa
@Thickness 12.7 mm
ASTM D2240
 
Processing PropertiesOriginal ValueComments
Gel Time <= 0.917 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
Covestro Baydur® 684 Polyurethane Structural Foam RIM, Density 15 pcf

PCOVEST0090 / 201873

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.